[TheForge] welding cast iron
Peter Fels And Phoebe Palmer
artgawk at thegrid.net
Tue Dec 13 02:25:31 EST 2005
That feed ratchet arm came broken on my post drill too.
Could it be that that is an easily reparable weak link in the
system and that replacing it with a stronger forged one will do
more damage when the next screw up happens?
A normal oxy-acet torch and cast iron flux with the cast rods
works fine with sufficient preheat on cast iron.
Brazing rod shrinks at a different rate than the cast and can add
stress to long joints.....Pete F
Patty Draper/Bill Robertson wrote:
> I'm logging on late on this topic. Has anyone mentioned the Henrob 2000
> torch. With cast iron welding rods that are available it welds cast
> iron great with just low pressure ocyactelyene. Just Google Henrob
> torch and you will find tons of info. Bill
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
>
More information about the TheForge
mailing list