[TheForge] eucalyptus charcoal
kevin donahoe
flyinpig at go-concepts.com
Sun Aug 21 20:59:20 EDT 2005
OK, looked it up, gray cast iron runs 2.8-3.5%... can't find what the pig
iron is in my book.
I'd say that's a lot of eucalyptus tree in that pig.
Kevin D
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of Peter Fels And
Phoebe Palmer
Sent: Sunday, August 21, 2005 4:05 AM
To: Sponsored by ABANA
Subject: Re: [TheForge] eucalyptus charcoal
This leaves a lot of carbon unaccounted for...
or they are producing a lot more iron per unit charcoal than I'd
have guessed....PF
kevin donahoe wrote:
> about 2%?
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net]On Behalf Of Peter Fels And
> Phoebe Palmer
> Sent: Saturday, August 20, 2005 4:00 AM
> To: Sponsored by ABANA
> Subject: Re: [TheForge] eucalyptus charcoal
>
>
> Just how much carbon do they stuff into those pigs anyway?
>
> schade at acegroup.cc wrote:
> > At the Nucor website
> >
http://nucor.com/enviropages/articles/03- RenewableCarbonSource
they show
> > the "Net Loss to the
Environment" as 1.1 tons of CO2 per ton of Pig Iron
> > using eucalyptus charcoal. v. 2.2 tons of CO2 per ton of Pig
Iron using
> > "the traditional method".
> >
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list