[TheForge] Forge is up!
Rob Fertner
rfertner at cox.net
Thu Aug 11 11:03:21 EDT 2005
Dang. I can't find the copy I printed off few years back when someone
printed the Railroad specs for spikes. HC means high carbon (when
compared to previously used spikes) If there's an additional "C" on the
head, then copper has been added to the steel mix. My memory is fuzzy on
this part, I thought the specs said minimum carbon of .30%. The non-HC
spikes were around .20% carbon.
Anyway, unless there's something brand new being used, I don't believe
spikes get up to .50% carbon.
Rob
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Dan Tull
Sent: Thursday, August 11, 2005 8:06 AM
To: munlaw2 at hcsmail.com; Sponsored by ABANA
Subject: Re: [TheForge] Forge is up!
The spec data sheet I saw showed
HC to have a maximum carbon content of .30%.
Yes there is documentation, somewhere.
I didn't catch where he "steeled" the spikes.
----- Original Message -----
From: "Ron Childers" <munlaw2 at hcsmail.com>
To: "'Sponsored by ABANA'" <theforge at mailman.qth.net>
Sent: Thursday, August 11, 2005 6:49 AM
Subject: RE: [TheForge] Forge is up!
Dan,
Is there a spec sheet on this? I have heard the newer rr spikes,
so-called
"high carbon" are 1050.... I also heard the "HC" on the head means
"highway
crossing"; supposedly harder steel. This came from a self-ordained spike
expert. I have some really old ones that are wrought iron and a bunch
with
no markings which are purported to be mild steel. The smaller spikes are
definitely not hc. Anyway, Kent did it right by "steeling" the spike
with
real high carbon steel.
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Dan Tull
Sent: Wednesday, August 10, 2005 9:24 PM
To: kent; Sponsored by ABANA
Subject: Re: [TheForge] Forge is up!
Mild steel 30 pts. carbon MAX.
----- Original Message -----
From: "kent" <kent at cerakko.com>
To: "forge mail" <theforge at mailman.qth.net>
Sent: Wednesday, August 10, 2005 9:16 PM
Subject: [TheForge] Forge is up!
Had a great time at the OBG meeting last Saturday; went home and fired
up
the forge. Heated up some railroad spikes and a broken file, then beat
on it
for a while. Drew out a tang and forged in some bevels for a nice little
knife...maybe a skinner. (LOL) It do have a bit of curve to it, but I'll
straighten it out.
Have a question for ya'll, though. What kind of steel do they use to
make
railroad spikes?
Thanks,
Kent White
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge