Mild steel 30 pts. carbon MAX.
----- Original Message ----- 
From: "kent" <kent at cerakko.com>
To: "forge mail" <theforge at mailman.qth.net>
Sent: Wednesday, August 10, 2005 9:16 PM
Subject: [TheForge] Forge is up!


Had a great time at the OBG meeting last Saturday; went home and fired up 
the forge. Heated up some railroad spikes and a broken file, then beat on it 
for a while. Drew out a tang and forged in some bevels for a nice little 
knife...maybe a skinner. (LOL) It do have a bit of curve to it, but I'll 
straighten it out.

Have a question for ya'll, though. What kind of steel do they use to make 
railroad spikes?

Thanks,

Kent White
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________






More information about the TheForge mailing list