I have used clear coat over this product and also ceramic chrome wax and  
glow, with good results. I did some cabinet hard wear several years ago and they  
are holding up well. Once the product is put on only heat or a wire brush can 
 remove it. By mixing colors I am able to obtain fall colors on leaves. 
Gilders  paste offers a larger assortment of colors than the ceramic chrome (they 
have  7). Ceramic chrome is available at most ceramic supply stores for about 
$3.50 a  jar. You must remember that a little goes a long way, too much and 
your project  becomes painted garbage. It is easily removed, so try some. I apply 
with my  finger or a soft brush is fine also. Ralph Neumeister  WRABA