Your 485 lbs/cu. ft. is closer than my 0.3 pounds per cubic inch (0.28 would 
be better)  then it depends on if you are buying or selling (smile).  If the 
price is right sounds like a good table.
Dave
----- Original Message ----- 
From: <debmiller at fuse.net>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Tuesday, April 26, 2005 7:23 AM
Subject: Re: [TheForge] table weight


> Assuming it's solid and using 485 lbs/ cu.ft., roughly 5363 lbs.
>
>>
>> From: SRiverF at aol.com
>> Date: 2005/04/25 Mon PM 08:01:46 EDT
>> To: theforge at mailman.qth.net
>> Subject: [TheForge] table weight
>>
>> I have someone selling me a table for the scrap weight, Can anyone tell 
>> me
>> what a table 14' X 7' - 7" x 1& 1/4" thick would weight?
>>
>> /Thanks
>> Mike IVey
>> Savannah River  Forge
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login:  blacksmithblacksmith at hotmail.com
>> password:  anvil
>> ___________
>>
>>
>>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
> 


More information about the TheForge mailing list