I'm in the process of making some hot cut-off hardies for my anvils. and I
figured, since I've seen them both ways, I'd ask you guys about your
preferences, and why.I'm using a busted leaf spring for the metal.

Do you suggest single or double bevel, and why?

Whichever you suggest what angle is your preference for the cut- off edge?

Does this change if you're making a half round?