[TheForge] Pure Iron and 00Fe
April & Bill Clemens
newky2 at dejazzd.com
Wed Apr 20 21:36:52 EDT 2005
All,
I've checked and found out there is still Pure Iron and 00Fe available
from Roger Duncan's Estate.
Here's what's available and a chance to get some. Let me know.
Pure Iron and 00Fe Inventory from Roger Duncan's Estate
While there have been several inquires no one has purchased the
remaining stock of Pure Iron and 00Fe that Roger Duncan had. Here is
what is available:
Pure Iron
(approx 7 foot lengths the actual lengths vary and the cost will be
based on the actual weight at $1.25/LB)
SIZE LGTHS Ft W/LGTH $/LGTH Want LGTHS
0.25 X 1 10 70 5.95 $7.44 _______
0.25 X 1.5 6 42 8.93 $11.17 _______
0.25 X 1.75 8 56 10.42 $13.03 _______
0.25 X 2 8 56 11.91 $14.89 _______
0.375 X 1.25 15 105 11.17 $13.96 _______
0.375 X 1.625 5 35 14.51 $18.14 _______
0.375 X 1.75 4 28 15.63 $19.54 _______
0.4375 X 3 4 28 31.26 $39.08 _______
0.5 X 0.75 15 105 8.93 $11.17 _______
0.5 X 1 12 84 11.91 $14.89 _______
0.5 X 1.25 4 28 14.89 $18.61 _______
0.5 X 1.5 14 98 17.86 $22.33 _______
0.625 Round 32 224 17.31 $9.13 _______
0.75 Square 18 126 13.40 $16.70 _______
0.75 X 1 1 7 17.86 $22.33 _______
0.8125Round 1 7 2.35 $15.44 _______
0.8125 X 1 1 7 19.35 $24.19 _______
1 Round 5 35 18.71 $23.38 _______
1.25 Round 16 112 29.23 $36.54 _______
OO Fe (5 foot lengths except for coil)
0.25 X 0.3751276LB coil 4000 .32 $.40 per ft _______ FT
0.25 X 0.75 2700 13500 3.19 $3.99 _______
0.25 X 1 1500 7500 4.25 $5.32 _______
Name:______________________________
Phone:_____________________________
Email:
_____________________________
If you'd like to purchase some of the above, contact me and I'll put a
consolidated list together and then make arrangements for a date and
time to pick it up and bring it to the BGCM shop at the Carroll County
Farm Museum prior to Blacksmith Days 21 May 2005.
Bill Clemens (570)568-2158 newky2 at dejazzd.com