I have spring shop drops, lumber yard bandsaw blade, a couple of axles and other odds and ends, However, none of them is large enough for a power hammer die.  My point was not to be snide or demeaning, but to help those professional smiths out there remember some of us are not full time smiths, with well stocked smithies.

-Chris K.

----- Original Message -----
From: "Dan Tull" <dantull at numail.org>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Subject: Re: [TheForge] Super Quenched Dies?
Date: Wed, 20 Apr 2005 10:53:53 -0400

> 
> I detect a flame war brewing.
> 
> Maybe you should change your priorties then. There is plenty of 
> tool steel available free if you will "lower" yourself enough to  
> ask.
> But then you probably wouldn't go dumpster diving either, huh.?
> 
> ----- Original Message ----- From: "Chris Kilpatrick" <crimsonkil at lycos.com>
> To: <munlaw2 at hcsmail.com>; "Sponsored by ABANA" <theforge at mailman.qth.net>
> Sent: Wednesday, April 20, 2005 10:47 AM
> Subject: RE: [TheForge] Super Quenched Dies?
> 
> 
> Rob gunther got a 48 rockwell all the way through a 1" bar, I'd say 
> the quench goes pretty deep.  there are some of us here who have a 
> forging budget of about $25/week, because it is a hobby, so 'good 
> steel lying around' does not describe my shop.
> 
> 
> 
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________



It is I who formed the blacksmith, 
who fans the flame into a fire and
fashions a weapon fit for it's work.

-- 
_______________________________________________
NEW! Lycos Dating Search. The only place to search multiple dating sites at once.
http://datingsearch.lycos.com



More information about the TheForge mailing list