[TheForge] Super Quenched Dies?

magichammer dave at magichammer.net
Mon Apr 18 23:14:36 EDT 2005


I have a 50# / 75# Kinyon hammer with 4" square flat dies made of 43-40
used daily, never been heat treated, still in great shape after years of 
use.
see here: http://magichammer.freeservers.com/page5.html

dave m

----- Original Message ----- 
From: "Carl Tappan" <carlt at bluetoad.org>
To: <theforge at mailman.qth.net>
Sent: Monday, April 18, 2005 3:41 PM
Subject: [TheForge] Super Quenched Dies?


> Hey all, I am wondering if anyone has any experience with super quenched
> power hammer dies? Kinyon, about 35 lbs ram weight, I am thinking just
> flat dies but would also like to make some other styles. It seems
> reasonable to me, but I don't trust my own judgment. Anyway, feedback
> solicited.
> Thanks,
> Carl Tappan
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
>
> -- 
> No virus found in this incoming message.
> Checked by AVG Anti-Virus.
> Version: 7.0.300 / Virus Database: 266.9.13 - Release Date: 4/16/2005
>
> 



-- 
No virus found in this outgoing message.
Checked by AVG Anti-Virus.
Version: 7.0.300 / Virus Database: 266.9.13 - Release Date: 4/16/2005



More information about the TheForge mailing list