You can get fairly close (with a little math) by taking 12"x12"x1/4" as 
10 pounds. An easy one to remember when you're at the scrapyard.

Steve

Phlip wrote:
> Anybody know where, on line, I might be able to find a table of steel weight
> per running foot? I need to buy some stock, and since they price it by the
> weight, and I figure out how much I need by the foot, I thought it might be
> helpful if I knew what the conversion is.
> 