On Apr 7, 2005, at 9:56 AM, Jay Hayes wrote:
> Bob,
>
> ITC-100 will improve the amount of radiant heat reflected from the
> interior surfaces of the forge. This will help the forge run hotter
> and conserve fuel. It can be used on cast able refractory, fire brick,
> ram able refractory, as well as ceramic fiber. ITC-100 is more
> expensive then the other coatings mentioned, but performs better at
> higher temperatures. It pays for itself in short order in fuel savings
> alone, not to mention the extended refractory life. We like it so
> much, we include ITC-100 with all of our forge kits.
>
> Jay Hayes
> C. J. Products Inc.
>
>
>
> Schade wrote:
>
>> would a coating of satanite/plistex/itc etc. improve the heat of a
>> forge that was lined with a castable refactory?
>>
>> Bob
>> _____