I never figured on a big difference in the kaowool or durablanket. I
know there are different densities. even with different densities, they
are all rated around 2300 F. but loose heat slower the denser( more
dense) the material. perhaps you got a denser durablanket than the
kaowool. I got a freebe also I don't know what I have. just that I
can't quite get to weld heat. I do need the coating to stob the
insulation from detiorating away and causing the hazzard of the
particulates in the air.