Larry Zoeller zman59 at earthlink.net
Fri Apr 1 23:03:54 EST 2005


To All,
The Plistix 900F has a 2800 degrees rating.

Thanks,
Larry Zoeller
4312 Lahnna Dr.
Louisville, KY 40216
zman59 at earthlink.net
www.geocities.com/zoellerforge


> [Original Message]
> From: Jeffrey Polaski <jpolaski at rgs.uci.edu>
> To: <zman59 at earthlink.net>; Sponsored by ABANA <theforge at mailman.qth.net>
> Date: 4/1/2005 4:30:17 PM
> Subject: RE: [TheForge] local source of ITC 100
>
> I wish I would have known about the Plistix, I just bought a bunch of
> ITC-100. Does the Plistex work to the same temperatures? 
>
>
>
> Jeff Polaski
> RGS Webmaster
> (949) 824-6363
>
> "The ant has made himself illustrious
>  Through constant industry industrious.
>  So what?
>  Would you be calm and placid
>  If you were full of formic acid?" 
> 			-Ogden Nash
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Larry Zoeller
> Sent: Wednesday, March 30, 2005 6:31 PM
> To: theforge
> Subject: Re: [TheForge] local source of ITC 100
>
>
>
> To All,
> I sell two different materials that are a great replacement for ITC 100
> at a substantial savings, I have the Plistix 900F and QF-180 and they
> both have the high thermal reflective properties that you need.  And if
> you feel like driving to Kentucky you can pick it up also. The following
> URL will have more information.
> http://www.geocities.com/zoellerforge/flare.html
> I try not to push my products an the list, but with this thread I feel
> it is valuable information that could be added. Thanks, Larry Zoeller
> 4312 Lahnna Dr. Louisville, KY 40216 zman59 at earthlink.net
> www.geocities.com/zoellerforge
>
>
> > [Original Message]
> > From: S. Pohlman <ajarrod at voyager.net>
> > To: Schade <schade at acegroup.cc>; the forge <theforge at mailman.qth.net>
> > Date: 3/30/2005 6:21:57 PM
> > Subject: Re: [TheForge] local source of ITC 100
> >
> >  Centaur forge is great for alot of things however they do not carry 
> > any
> > ITC 100 or other refractory material. just rebuild kits for the forges
>
> > they sell. when I called  they hadn't even herd of it.
> >    someone mentioned plistix how does that compare? or the fibrefrax
> 180 
> > blue
> >
> > Schade wrote:
> >
> > > Stu,
> > >
> > > You can't be much more than a hour from Centaur if you wanna buy in
> > > person. My map shows about 40 miles (Lake Zurich, IL to Burlington, 
> > > WI). I would consider that pretty local for a somewhat specialized
> item.
> > >
> > > Another online source would be Larry Zoeller also on this list.
> > >
> > > Bob
> > > ______
> > >
> > >
> > > On Mar 29, 2005, at 5:09 PM, S. Pohlman wrote:
> > >
> > >> I live in the North East corner of Illinois.  Lake Zurich in Lake
> > >> county to be exact. Centaur forge is great for most stuff but I am
> re 
> > >> doing my gas forge and want to find a local source for  itc100 
> > >> refractory. any help would be a great . I have seen it for sale on 
> > >> the net but prefer to buy in person.
> > >>
> > >> Stu
> > >>
> > >>
> > >
> > >
> > >
> >
> >
> > _______________________________________________
> > Manage membership or unsubscribe at: 
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is http://www.photoaccess.com
> > Login:  blacksmithblacksmith at hotmail.com
> > password:  anvil
> > ___________
> >
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>




More information about the TheForge mailing list