Farm supplie stores carry it. It is used for cleaning out milk lines. It
sells there for far less than the chemical companies. (Or for the really
dilute phosphoric acid get Coke or Pepsi).

> Where do you get phosphoric acid? How much does it cost?
> Darrell



More information about the TheForge mailing list