At 23:40 09/13/04, you wrote:
>Which burner system are you using? I've read about and looked over a bunch
>of descriptions and drawings over the last couple years and I seem to recall
>one that was primarily ductwork.
No duct work. That sounds like a Mother Earth News drip style
thingie. I'm working on an atomizer/nebulizer type along the lines of a
Babington burner. It's exactly the same, only different.
Dave Brown
Heritage Smithing