PCB Cleaner works faster diluted. Up to 50% water.
Aquarium ariator bubbling speeds and evens out process.
dan tull
georgia
abba, afc, S.C. psba, obg,sofa
----- Original Message -----
From: <PlumDon at aol.com>
To: <theforge at mailman.qth.net>
Sent: Friday, September 10, 2004 10:42 AM
Subject: Re: [TheForge] Etchant strength
>
> In a message dated 9/10/2004 8:38:31 AM Eastern Standard Time,
> irontree at visi.com writes:
>
> I purchased some etchant from Radio Shack. Am I supposed to use this
stuff
> at
> full strength or am I supposed to dilute it? Anyone?
>
>
>
> The etchant Rob Hudson, a noted East Coast knifemaker uses is ferric
> chloride. It is most conveniently available from Radio Shack where it is
called PCB
> Etchant Solution. It is most effective when it is mixed with 5 parts water
to
> 1 part etchant. Rob thinks it would probably be equally effective at an 8
to
> 1 mix. The timings in the echant are dependent on your personal tastes.
In a
> damascus blade I did I used three 8 minute cycles. It was held in the
> etchant for 8 minutes, removed and tooth brushed clean with a bit of
water,
> re-immersed for 8 mins and cleaned and then once again.
>
> Don Plummer
> Plummer Design Works
> 392 Hallman Mill Road
> Phoenixville, PA 19460
> 610-495-5058
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list