In a message dated 9/10/2004 7:38:33 AM Central Daylight Time, 
irontree at visi.com writes:
Also what do I do with the stuff once it it no longer usable.  I figure it 
will
last a long time since I don't make that many blades, but I also know that 
this
stuff does eventually weaken with use.....How do I dispose of this safely?  I
grow food on my property and I have shallow well, so dumping it is right
out...anyone?
How bout mixing with sodium bicarbonate to bring it to a a more neutral 
solution. then safer to deal with. 

Time enough for sleep in the grave.
Tod Estes.