Frederick:
You got 1/4" square hot rolled? I don't think they
make it any more. All I ever see is 1/4" cold rolled.
Some distributors carry 5 mm square hot rolled.
You're a lucky dog! Send me about 100 sticks of it,
would you?
Phil Rosche
Summerville, SC
> Frederick Faller wrote:
> > Just went to get some mild steel (1/2, 1/4, 3/8
> square
> > hot rolled A36). Price is coming in about $.90/
> lb. Is
> > this reasonable? I know the price has gone up
> > dramatically, but ...
> >
> > Frederick Faller
> >
> > =====
> > Frederick W. Faller
> > Shiloh Forge Ironware
> http://users.rcn.com/ffaller/SFI_web.htm
> > www.immerland.com
> >
> >
> >
> > __________________________________
> > Do you Yahoo!?
> > Yahoo! Mail Address AutoComplete - You start. We
> finish.
> > http://promotions.yahoo.com/new_mail
> > _______________________________________________
> > Manage membership or unsubscribe at:
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: blacksmithblacksmith at hotmail.com
> > password: anvil
> > ___________
> >
> >
> >
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
__________________________________
Do you Yahoo!?
Y! Messenger - Communicate in real time. Download now.
http://messenger.yahoo.com
More information about the TheForge
mailing list