[TheForge] MIG setup
Jerry Frost
frosty at customcpu.com
Thu Oct 28 12:56:02 EDT 2004
Thanks Dave.
Please disregard my last bit of wrongness.
Seems this is one of those mental block things. Many years ago somebody
who'd been welding all their life told me the even/odd significance and even
though I've been corrected before I can't seem to get it out of my head.
<sigh>
Frosty
------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks
Meadow Lakes, AK.
----- Original Message -----
From: "Dave Brown" <quahog at netnet.net>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Monday, October 25, 2004 5:38 AM
Subject: Re: [TheForge] MIG setup
> At 23:40 10/24/04, you wrote:
> >6013 is AC rod and if it runs fine you almost undoubtably have an AC
> >machine. Odd number rods are AC, even are DC
> >
> >Go to the welding supply and get an AC 70xx rod. Get a couple lbs of
> >different rods to try.
> >
> >Frosty
>
> 6013 is AC or DC. The odd/even rule of thumb applies more to whether you
> not you a rod is suitable for AC, but all rods can be run DC. See below.
>
>
> ELECTRODES AND CURRENTS USED
>
> * EXX10 DC+ (DC reverse or DCRP) electrode positive.
> * EXX11 AC or DC- (DC straight or DCSP) electrode negative.
> * EXX12 AC or DC-
> * EXX13 AC, DC- or DC+
> * EXX14 AC, DC- or DC+
> * EXX15 DC+
> * EXX16 AC or DC+
> * EXX18 AC, DC- or DC+
> * EXX20 AC ,DC- or DC+
> * EXX24 AC, DC- or DC+
> * EXX27 AC, DC- or DC+
> * EXX28 AC or DC+
> * NOTE The EXX1X and EXX2X designate rod suitable for 1=All
> position, 2=Flat and overhead, 3=Flat only.
> *
>
> My favorite rod for mild steel is E7018. Some rod manufacturers make a
> 7018-AC which is for AC use only and works very well there.
>
> Dave Brown
>
> "Always vote for principle, though you may vote alone, and you may
> cherish the sweetest reflection that your vote is never lost."
> - John Quincy Adams
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list