[TheForge] angled tenons

Wayne Ackman LongHollow.Forge at starband.net
Sun Oct 24 22:38:22 EDT 2004


My current project calls for one bar with a tenon
piercing another bar at a 25 degree angle.
I haven't done that before.  thinking about it,
it seems I need to make an angled monkey tool
to set the shoulder. But how do you isolate the tenon?
just do it as typical and let the monkey tool angle it?
doesn't seem like that would do it and look good.
am I on the right track?

Wayne