> In basic terms it was a matter of heating the opposite side and
> then cooling with water and shrinking the "dimple".
>
> Ray
> Cincinnati
That sounds kind of fun...so, the heat goes in the concave side, right?
Then (I'm guessing here) heat until it expands and becomes straight, and
stop it in time...