That sounds WAY too expensive.
My 4X8 X 1/2 NEW was $130
dan tull
georgia
abba, afc, S.C. psba, obg,sofa
----- Original Message -----
From: "Gladish Family" <gladish at cnw.com>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Friday, October 15, 2004 9:56 AM
Subject: [TheForge] scrap plate steel
> Is there a way to straighten steel plate?
>
> I need to extend a welding table, so went to the local supplier and priced
> a
> new 4x5, 1/2". For new steel it's ninety-some cents a pound, about $350...
> But wait! There's a four by five chunk of 1/2" out back! About $100.
> Unfortunately it must have had something sitting on it, because it's
> dished,
> oh, maybe 3/8. Not that much, but the point is to have a dead flat surface
> to do layout.
> If it weren't so thick, I'd just build the frame and plug weld it, force
> it
> to be straight, but 1/2" seems too burly.
> Thanks for any suggestions,
> Andy g.
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list