[TheForge] rpm/horsepower
gblacksmith
gblacksmith at alamedanet.net
Thu Oct 7 11:55:31 EDT 2004
Folks: This thread is a good one! I have a 2hp Bader III, VS 2"x72" that
will grind heat treated stainless all day, barely getting warm. I use a 5/8
hp grinder with a 1"x42" belt at 1750 rpm for handle shaping. I also use a
1hp 8" at 3450 for profiling,as it is cheaper to use than belts. It seems
that there is a place for all of them, based on performance and cost.
Grant
----- Original Message -----
From: "Ries Niemi" <rniemi at fidalgo.net>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Wednesday, October 06, 2004 2:16 PM
Subject: Re: [TheForge] rpm/horsepower
>
> On Wednesday, October 6, 2004, at 10:33 AM, Schade wrote:
>
>>
>> I need a new bench grinder. The one I have is 1/2 HP 1750 RPM.
>> It seems like everything I have seen is higher horsepower and 3600
>> RPM. Is this marketing? Is a 1/2 HP 1750 RPM the same (torque)
>> as a 1 HP 3600 RPM?
>>
>> Bob
>>
>>
>
> Where the heck did you get a 1750 rpm bench grinder?
> Grinding wheels are designed and rated in surface feet per minute, with
> the average stones wanting to run around 5000sfpm. A 6" grinding wheel on
> a 1750rpm grinder is running at about half that- too slow, in other words.
> Commercially, almost all bench grinders are 3450 rpm until you get up to
> the big dogs- say 12" or 14", at which point they drop down to 1750.
> Now if you are gonna use this for buffing, or wire brushing, that might be
> different. But for grinding, in a 6" or 8" size, you want 3450, and thats
> what they make.
> As far as torque goes, yes, its true that a slower motor has more torque
> for the same horsepower. But you need the speed, so you do need a bigger
> motor. I have a 1 1/2hp Jet that I am quite happy with- cant seem to slow
> it down.
>
> If you are wet grinding woodworking tools, of course, throw all this out
> the window, and buy a special machine for that. But for general purpose
> sharpening and grinding, 3450 is right.
>
> ries
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list