I would say on the diamond would be stronger because on the square would
put the corner closer to the edge. and thus thinner, though I think the
difference would be minor depending on the direction of the forces.
mike
At 01:51 PM 10/1/2004, you wrote:
>In slitting and drifting a square hole,
>since no metal is lost,
>will it make a difference in strength if the hole is square to the side
>or on the diamond?
>
>
>dan tull
>georgia
>abba, afc, S.C. psba, obg,sofa
>_______________________________________________
>Manage membership or unsubscribe at:
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: blacksmithblacksmith at hotmail.com
>password: anvil
>___________
Mike Linn
Artist Blacksmith
McCalla, AL
AFC Webmaster
http://afc.abana-chapter.com
"Don't worry Chief, I can stand the torture if they can stand the screaming."
- Maxwell Smart, Secret Agent 86
______________________________________________________________________
More information about the TheForge
mailing list