[TheForge] Possible return of Pure Iron to the USA
Schade
schade at acegroup.cc
Tue Nov 9 17:41:36 EST 2004
Phil,
Sorry. Didn't mean to sound rude.
I think this is why pure iron went out of business the
first time. It might be better but not better enough to
matter. But again I haven't tried it. I'll mail you direct
about buying a piece.
Bob
___
On Nov 9, 2004, at 1:54 PM, Phil wrote:
> Bob:
>
> As they say in the north "you talkin' to me?"
>
> Personally, the reason I don't use it is that it's all
> standing up in the corner, and I always forget to use
> it. I like cold rolled just fine.
>
> Phil
More information about the TheForge