	Definitely do it in stainless steel.  It will last forever without
	any maintenance.  You can patinate it.  There are patinas available
	but if you can get a hold of cat pee, that is the best of all, no
	joke.  It will turn stainless steel absolutely JET black.


Cat pee: I have plenty of cats; house cats, barn cats, yard cats, kitty cats
& waumpus katts. Your mission, should you decide to accept it, is to harvest
said cat pee. (And bring your own jug). Ron C