That was not meant in a derogatory manner; it was a compliment.  I'm the one
to apologize if it came out sounding otherwise.  I've been told my sense of
humor is sometimes a bit off the norm.  I really enjoyed the info, and like
the stuff on the steel drums, as well.  When I said that about it only
counts when you build it, I was not trying to belittle the use of research,
whether on the Web, in the library, or from other people in the field.
Research and planning are very useful in reducing the chance of error when
you do actually build whatever you're working on.  My main point was that
until it gets off the drawing board and onto the anvil, it's still theory;
until you actually try it, you don't know it'll work.  I've had many
projects look real good in theory, with proper engineering and measurements
in the drawings, etc.  Then when I actually build the thing, it won't work.
Murphy's Law states that it will never work the first time.  Good planning
and research can never beat Murphy's Law, but they can sure reduce the
number of tries before it does work.

Again, apologies if I sounded snotty; I didn't mean to.

Mike Murphy 

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Dan Hayes
Sent: Wednesday, May 05, 2004 5:39 PM
To: [email protected]
Subject: RE: [TheForge] Triangles

Didactic and pedagogical? Sorry I came off that way. And I apologize if I
offended anyone, which I think I might have since I seemed to have killed
the thread. I really didn't mean to do that.

Anyway, if you want something more entertaining, try this link:
http://www.sciencenews.org/pages/sn_arc98/10_10_98/bob2.htm
It's about the metallurgy of Caribbean steel drums, and it does address the
effect of carbon content and heat treatment on the sound of the drum.

Dan

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Michael H. Murphy
Sent: Wednesday, May 05, 2004 6:03 PM
To: [email protected]
Subject: RE: [TheForge] Triangles

Dang! I though I was getting didactic and pedagogical.  But he's right;
different steels have different qualities -- in malleability, hardness, and
acoustics.

I agree with researching it on the Web, for all kinds of ideas and
techniques.  But it still doesn't count until you've actually put it
together and listened to it.

Mike Murphy

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Daniel T. Hayes
Sent: Tuesday, May 04, 2004 8:37 PM
To: [email protected]
Subject: RE: [TheForge] Triangles

Bob,

The acoustic properties of steels are affected by many factors, and
"scientific proof", along with a lot of specific data is available if you
know where to look. You might want to consider looking into a metallurgical
reference book such as Metals Handbook or a text on ultrasonic inspection.

The two acoustic properties that come to mind as major players in
determining the sound of a triangle or bell are acoustic velocity
(longitudinal/compression, transverse/shear and surface)and acoustic
impedance. You can find this kind of data tabulated in metallurgical texts,
and if you do a web search, I'm sure you could come up with a number of
narrowly focused research papers on the subject. In any event, you'll find
that carbon content, alloying elements, heat treatment and deformation/work
(both cold and hot) all play significant roles. In each case, you'll find
that the answer lies in how each of these factors affects the crystalline
structure(s) of the metal. An FCC lattice can be expected to transmit sound
differently from a BCC lattice or a highly strained martensitic structure,
for example. Throw in the fact that most steels are a mixture of phases and
the problem gets really complex. Acoustic impedance is probably the most
complicated acoustic property of all. You're best bet is probably to
research metallurgical texts for information on acoustic properties.

Dan

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of [email protected]
Sent: Tuesday, May 04, 2004 7:48 PM
To: [email protected]
Subject: Re: [TheForge] Triangles

Thanks for the reply Steve. But what I am really
interested in is the scientific proof that says that
using higher carbon steel produces a different
ring than lower carbon steel and also why quenching
would affect the ring. These thoughts are often
presented as a given. If the proof is that common
it should be easy to show. Listening to various samples
is  subjective.

Bob
____


On May 4, 2004, at 5:55 PM, Steve Smith wrote:

> Bob, I think you have a very good point (in the absence of data at 
> this end also). Hardening the steel affects yield point, not elastic 
> bending.
>
> This should be pretty simple to try. I'd do it myself, but I'm still 
> trying to get my chimney up on the new shop--still no forge here. If 
> someone trys it, the listening test should be blind: a helper does the 
> ringing of the triangles, and the listener doesn't know whether it is 
> a hardened triangle or a soft one. Several (random) trials of each. 
> Who's going to volunteer?
>
> Steve Smith
>
> [email protected] wrote:
>
>> Is it really the hardness or carbon content of the steel that changes
>> the tone or is it the shape?
>> I think the shape. Small differences between one triangle and another
>> may change the tone but I think the tone is not affected by the carbon
>> content or the quenching. Super or otherwise.
>> This opinion is just an opinion. I have no actual data to confirm or 
>> deny.
>> If you do have actual data (not anecdotal) I would like to see it.
>> Bob
>> ___________
>>> At 15:57 05/03/04, you wrote:
>>>
>>>> Made a few triangles - I found that mild steel works
>>>> fine, but you get a much better ring if you quench the
>>>> corners in superquench. Really improves the tone and
>>>> intensity.
>>>>
>>>> FWFaller
>> _______________________________________________
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login:  [email protected]
>> password:  anvil
>> ___________
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>

_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  [email protected]
password:  anvil
___________





_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  [email protected]
password:  anvil
___________


_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  [email protected]
password:  anvil
___________





_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  [email protected]
password:  anvil
___________