You could fill with an epoxy copper powder goo and electroplate with a brush
type plating system. Also solder sand and electroplate.
http://www.caswellplating.com/kits/copper.htm
Mike McKim
----- Original Message -----
From: "Gladish Family" <[email protected]>
To: "Theforge" <[email protected]>
Sent: Sunday, March 28, 2004 12:27 AM
Subject: [TheForge] copper goo or paste
> Say, anybody know about some kind of copper colored filler paste- sort of
> like JB Weld for copper?
> I'm doing countertops in our home, and would like the seams to disappear
as
> much as possible.
> Thanks, everybody!
> Andy Gladish
>