[TheForge] cast iron welding

Bruce Freeman [email protected]
Thu Mar 18 08:39:02 2004


I'm no expert, but we did some comparable work on cast iron anvils
recently - "buttered" them with nickel rod, then welded on steel to
replace broken parts of the steel plate.  Seems to have worked quite
well.  Lower investment cost if you already weld.

Bruce
NJ

>>> [email protected] 3/18/2004 1:18:22 AM >>>
To-day I witnessed a demonstration on building up cast iron with a Ni 
spray.A torch is the method of delivery. A bottle of Ni (nickel)was 
screwed into this custom set-up.
11# of acetylene 20# oxy. The torch has a trigger, when pressed the
powder comes out with the flame. The torch tip looks like a welding tip

with a O2 trigger on it.

The piece was one half of an old crank style blower. One of the ears
was
broken off where the two half s screwed together. First the piece was 
heated up to about 400* F. Then this slick
torch started to do its thang. The end product is a brandy new shiny
tab. He wanted $ 500.00 for the set-up. I can post pics if you want to

see the process. I thought it was rather pricey.
If I did lots of cast welding and happen to have 500 clams I'd have
one.

Kenny O



_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge 
theforge mail list group photo site is
http://www.photoaccess.com 
Login:  [email protected] 
password:  anvil
___________