......I know that they can be hard as hell to drill and that they have hard
spots.
dave m
----- Original Message -----
From: <PlumDon at aol.com>
To: <theforge at mailman.qth.net>
Sent: Monday, June 28, 2004 3:42 PM
Subject: [TheForge] Bed frame steel
> Anyone have any idea what bed frames are typically made of? They spark
test
> out with a fair quantity of carbon and will harden. I always assumed they
were
> whatever junky stuff might be available but all the frames collected over
the
> years consistently test out at relatively high carbon.
>
> I'm cutting some up to make shelf supports for steel stock not making
samurai
> swords or the like. Just a casual concern about cooling quickly in water
> after some mig welding.
>
> Kindest regards
>
> Don Plummer
> Plummer Design Works
> 392 Hallman Mill Road
> Phoenixville, PA 19460
> 610-495-5058
> _______________________________________________
More information about the TheForge
mailing list