[TheForge] Snarling iron pics
Demon Buddha
[email protected]
Tue Jan 27 21:23:01 2004
That's a pretty decent looking iron you have there, Mike.
Try superquenching it to make it springier if it is too mushy.
-Andy
----- Original Message -----
From: "Mike Spencer" <[email protected]>
To: <[email protected]>
Sent: Tuesday, January 27, 2004 6:09 PM
Subject: [TheForge] Snarling iron pics
>
> Here are a couple of pics if my attempt at a snarling iron.
>
> http://home.tallships.ca/mspencer/snarl.html
>
> - Mike
>
> --
> Michael Spencer Nova Scotia, Canada .~.
> /V\
> [email protected] /( )\
> http://home.tallships.ca/mspencer/ ^^-^^
>
> --
>
>