On Thu, 22 Jan 2004, Kenny O. wrote:
kenny>
kenny> I have started to build the Sandia forge. The plans are from ABANA.
kenny> I posted some pictures of the sheet metal I bent today. The easy part
kenny> as far as I can tell. I am having a hard time finding the insulation board
kenny> around So. OR.
kenny> I thought I might use Kaowool and paint it with ITC-100.
kenny>
look for a pottery shop.
find a kiln shelf made from alumina.
use that for the bottom.
the pottery shop should also have the insulation board
since it is used for homemade kilns.
kaowool insulation board is a bluish-green before it is heated
the first time after that it turns white.
kenny>
kenny>
kenny> How does that sound?
kenny>
<snip>
kenny>
kenny> Kenny
kenny>
--
terry l. ridder ><>