John Emmerling wrote:
> 
> does anyone know what type of  steel is used for punches in ironworkers?
> i am replacing several broken ones and am thinking  about forging the
> broken ones for use with the air hammer or press. what heat treat+ temper?
> thanks

	I believe D2 is common.