[TheForge] tips for cleaning steel?
[email protected]
[email protected]
Fri Jan 2 11:13:01 2004
Jeff
Cold rolled can be worth the difference, especially with smaller stock, but
it does has some pitfalls of its own. Square stock is often semi-hardened for
use as key stock. The same can hold true for round stock use for pins. Just
something to be aware of.