[TheForge] Damascus warpage and blade rivets

Dan Tull [email protected]
Sun Feb 22 15:17:00 2004


Blades can warp if you don't quench them oriented North and South.

dan tull
georgia
abba, afc, S.C. psba, obg,sofa
----- Original Message ----- 
From: "Daniel Kretchmar" <[email protected]>
To: <[email protected]>
Sent: Sunday, February 22, 2004 2:55 PM
Subject: [TheForge] Damascus warpage and blade rivets


> Curiousity,
> 1.    Several of the last few blades I have done have warped during the
the
> hardening process.  I have attached the steps below.  What am I doing
wrong?
> 2. Anyone know where I can get the 2 part copper/brass rivets that have
end
> up having flat heads on booth sides of the knife handle?  I think one fits
> inside the other.
>
> Dan
> www.irontreeworks.com
> Steps
> 1. Make the billet
> 2. Anneal the billet
> 3. grind the blade and drill the tang
>
> ****This is where it warps*****
> 4. Harden (heat to orange and quench in water)
>    ****This is where it warps*****
>
> 5. Temper the blade (cover the edge in clay, heat back of knife to straw
> color, let cool
> 6. finish sand and polish.
> 7. dip in acid to release pattern
> 8. Attach handle (sand handle to fit)
> 9. sell for $14,000,000.00  :)
>
>
>
>
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>
>