[TheForge] Damascus warpage and blade rivets
Daniel Kretchmar
[email protected]
Sun Feb 22 14:53:00 2004
Curiousity,
1. Several of the last few blades I have done have warped during the the
hardening process. I have attached the steps below. What am I doing wrong?
2. Anyone know where I can get the 2 part copper/brass rivets that have end
up having flat heads on booth sides of the knife handle? I think one fits
inside the other.
Dan
www.irontreeworks.com
Steps
1. Make the billet
2. Anneal the billet
3. grind the blade and drill the tang
****This is where it warps*****
4. Harden (heat to orange and quench in water)
****This is where it warps*****
5. Temper the blade (cover the edge in clay, heat back of knife to straw
color, let cool
6. finish sand and polish.
7. dip in acid to release pattern
8. Attach handle (sand handle to fit)
9. sell for $14,000,000.00 :)