Ralph Sproul wrote:
> Roger, I've used a larger size liner than the wire I'm running, and
> the same size tip for hard wire(common steel wire used with gas) and dual
> shield wires(flux cored wire DESIGNED to run along with a shielding gas as
> well.
> The place one would use a larger tip than the wire being run(along
> with a larger liner) is in the use of flux cored wire. The reason for this
> is that the shielding gas acts as a cooling agent in regular mig process,
> but the Flux cored wires run hotter and usually slower in wire speed so the
> expanding wire tends to jamb more. This is especially true in the larger
> structural wires run at high amperages and at a somewhat slow wire speed on