>>Someone once told me that if you are using say .030 wire then you do not
>want
>>to use a .030 tip but the next larger size. In other words always use a
tip
one size larger that the wire you are using.
I must say I always use the same size wire as tip and have had no problems,
but then again I live in a very dry climate. Possible this recommendation
is
a solution for those with a pitting problem on their wire. Has anyone else
ever heard of this?
Roger Olsen
The tip is called a contact tip there is a camber in the wire that
causes the wire to have a continuous contact . A larger sized contact
tip than the dia. of the wire will cause sporadic arc,
burn back and really skew up a good weld. There is also a helical twist
to aid in the flow of current.
K.O.