[TheForge] Mig Wire
Roger Olsen
[email protected]
Thu Feb 5 11:19:00 2004
Someone once told me that if you are using say .030 wire then you do not want
to use a .030 tip but the next larger size. In other words always use a tip
one size larger that the wire you are using.
I must say I always use the same size wire as tip and have had no problems,
but then again I live in a very dry climate. Possible this recommendation is
a solution for those with a pitting problem on their wire. Has anyone else
ever heard of this?
Roger Olsen
________________
Dan Tull wrote:
> Dealers sell small felt "cylinders" ( split and clipped) impregnated :~)
> with oil that slides on before the drive.
> inexpensive , and helps about that much, too.
>
> dan tull
> georgia
> abba, afc, S.C. psba, obg,sofa
> ----- Original Message -----
> From: "Howell Steve" <[email protected]>
> To: <[email protected]>
> Sent: Thursday, February 05, 2004 9:51 AM
> Subject: RE: [TheForge] Mig Wire
>
> > re: mig wire corrosion
> >
> > One trick is to wrap a piece of scotch-brite around the wire with a
> clothes
> > pin- right after it comes off the spool. Fasten it so it won't get caught
> up
> > in your rollers.
> >
> > Steve
> >
> >
> > --- StripMime Report -- processed MIME parts ---
> > multipart/alternative
> > text/plain (text body -- kept)
> > text/html
> > The reason this message is shown is because the post was in HTML
> > or had an attachment. Attachments are not allowed. To learn how
> > to post in Plain-Text go to: http://www.expita.com/nomime.html ---
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: [email protected]
> > password: anvil
> > ___________
> >
> >
> >
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________