[TheForge] Mig Wire
Dan Tull
[email protected]
Thu Feb 5 11:04:01 2004
Dealers sell small felt "cylinders" ( split and clipped) impregnated :~)
with oil that slides on before the drive.
inexpensive , and helps about that much, too.
dan tull
georgia
abba, afc, S.C. psba, obg,sofa
----- Original Message -----
From: "Howell Steve" <[email protected]>
To: <[email protected]>
Sent: Thursday, February 05, 2004 9:51 AM
Subject: RE: [TheForge] Mig Wire
> re: mig wire corrosion
>
> One trick is to wrap a piece of scotch-brite around the wire with a
clothes
> pin- right after it comes off the spool. Fasten it so it won't get caught
up
> in your rollers.
>
> Steve
>
>
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
> text/plain (text body -- kept)
> text/html
> The reason this message is shown is because the post was in HTML
> or had an attachment. Attachments are not allowed. To learn how
> to post in Plain-Text go to: http://www.expita.com/nomime.html ---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>