[TheForge] allstate oxy-propane torch
Jerry Frost
frosty at customcpu.com
Mon Aug 16 00:23:35 EDT 2004
----- Original Message -----
From: "Clyde Wynia" <clyde at tznet.com>
To: "'Sponsored by ABANA'" <theforge at mailman.qth.net>
Sent: Sunday, August 15, 2004 4:38 PM
Subject: RE: [TheForge] allstate oxy-propane torch
> Not a discrepancy also because you were comparing Oxy/propane to
> oxy/acetylene. I was comparing the Allstates oxy/propane to another
> oxy/propane, the Harris that is the same exterior design, on/off trigger
> etc.
>
> Of course I was also using 30 psi oxy (I can get 60 psi at 94% purity
> with the generator, not significantly different than the bottled stuff).
>
> And Frosty I'd love to meet your mother etc. Sure hope they do make it.
>
> Clyde
>
94% is better than I thought, last I remember they were running around
90-91%. Maybe that was at higher PSI or just older generators. Purity isn't
as imortant as PSI when you're power heating anyway.
Another thing I forgot to mention in the cost comparison is the cost of
fuel. 20 lbs of propane is still under $10 and is the equivalent of 15, 100
cf bottles of acetylene though I don't have any idea what acet costs.
Mother's wanted to see fall in your neck of the woods for many years, it's a
family trip we never managed to make and she asked where to find you
herself.
I've already given them all the directions they'll need. Go to Marshfield
Wi. and ask anybody.
Once I know their itinerary I'll give you some warning though a Frost family
itinerary can be a hazy thing.
Frosty
------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks
Meadow Lakes, AK.
More information about the TheForge
mailing list