Anyone else had a chance to try/test out the cast steel anvils from Harbor  
Freight? Apparently they come from Russia. The one I played with was 110 pounds 
 and cost $79. The face was hard the table was soft and the horn was hard. I 
used  a 1-1/2 lb ball pein hammer to test with a moderate hit. The horn has 
about as  much shape as a log but otherwise, this could be a very usable hammer 
with a bit  of dressing up. 
 
Been looking for a demonstration anvil and this might be it. 
 
Any other experiences here. 