Steve Smith wrote:
>
> Too much preheat can cause problems. You can take the hardness out of
> parts of the face you aren't working on if you heat too high.
>
> I use 300F for preheat; 500 sounds pretty high. As you weld, the temp
> will probably go up from your preheat. If you get too high, you will
> lose your temper. :)
That's what I thought, but last month they were taking them
to about 500 and the faces seemed to have held their hardness.
I was surprised because prior times we held to 300-350.