Ralph, Thanks for responding. I think I'll just screw my dies down. Bob
___

>Bob,  I don't use slide in, but clamp on.  I find loose fitting dies not
>only are dangerous, but they double hit like you say, give mis-prints on the
>bounce, and aren't worth it.  Clamping something down for fixed accuracy
>works for me.
>
>Ralph
>----- Original Message -----
>From: <[email protected]>
>To: <[email protected]>
>Sent: Sunday, September 28, 2003 11:21 AM
>Subject: [TheForge] slide in dies
>
>
>> I know there have been comments made here in the past about slide in dies
>being used on powerhammers. If anyone has built these I'd like to read how
>you like them, how you made them etc. Can you use slide in for top dies too?
>How do you tighten them? Do the top dies (or bottom) slap when you hammer?
>If anyone has a picture they could post that would be great.
>>
>> Thanks.
>>
>> Bob
>>
>>
>> _______________________________________________
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login:  [email protected]
>> password:  anvil
>> ___________
>>
>>
>>
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login:  [email protected]
>password:  anvil
>___________