Nickel anti-seize will work but the petroleum base of it burns off upon
contact with the hot metal creating fumes and the fine nickel powder
in the stuff is easily inhaled and ingested and nickel is a known
carcinogen. So if you don't care about that kind of stuff then go ahead
and use the nickel anti-seize but the weld-r-white is very benign stuff
it is water based so no burning oil and the boron nitride is not
considered dangerous other than it is a bad idea to inhale any fine
dust no matter what it is.
Jim
On Thursday, September 18, 2003, at 05:00 AM, [email protected] wrote:
> Kevin,
>
> I've never used it but G Dixon wrote up a product review back in the
> Winter 1998 issue of The Hammers Blow.
>
> He gave "Saf-T-Eze" an excellent rating. He describes it as a "Nickle
> Anti Seize"..."Anti-Seize is a grease like substance."
>
> The review says in part...."I found it's greatest application as a
> very high temperature lubricant for slit, drift and closed die
> forging"..."The Anti-Sieze coated tooling did the same job in 1/3 less
> heats."
>
> I googled and found http://www.saftlok.com/safteze/
>
> If you try it let me know.
>
> Bob
> _____
>
>
>
>
>
>
>> All,
>>
>> I've heard of using MdS2 as an agent to keep punches/chisels from
>> sticking
>> in hot work. It is apparently a powder, would anyone mind sharing
>> their
>> experience/ recipes for using this stuff? Is it "better" than
>> graphite or
>> coal dust, etc?
>>
>> Kevin Donahoe
>> Flying Pig Forge
>> Morrow, OH
>> [email protected]
>>
>>
>> _______________________________________________
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: [email protected]
>> password: anvil
>> ___________
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>