I've never used it but G Dixon wrote up a product review back in the Winter 1998 issue of The Hammers Blow.
He gave "Saf-T-Eze" an excellent rating. He describes it as a "Nickle Anti Seize"..."Anti-Seize is a grease like substance."
The review says in part...."I found it's greatest application as a very high temperature lubricant for slit, drift and closed die forging"..."The Anti-Sieze coated tooling did the same job in 1/3 less heats."
I googled and found http://www.saftlok.com/safteze/
If you try it let me know.
Bob
_____
>All,
>
>I've heard of using MdS2 as an agent to keep punches/chisels from sticking
>in hot work. It is apparently a powder, would anyone mind sharing their
>experience/ recipes for using this stuff? Is it "better" than graphite or
>coal dust, etc?
>
>Kevin Donahoe
>Flying Pig Forge
>Morrow, OH
>[email protected]
>
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login: [email protected]
>password: anvil
>___________