[TheForge] heated anvil

Peter Fels And Phoebe Palmer [email protected]
Tue Sep 16 01:35:01 2003


Along the same line, Has anyone experimented with using an alloy that 
doesn't transfer heat as fast as steel, for hammer-die or press die 
faces?   Pete F

Dan Scheid wrote:

>always before forge welding
> I either work some projects or I heat up a hunk of steel and place on the
>anvil other wise I find it to be a #300 heat sink that takes the heat out of
>my weld before I can hit it
>Dan Scheid
>"You ask a mare.
>You tell a gelding.
>You have a conversation with a stallion"
>Author unknown
>www.home.earthlink.net/~chevalvolant/flyinghorseforge.html
>  
>
>>Has anyone experimented with a heated anvil surface? This would make
>>    
>>
>welding
>  
>
>>and working on small pieces much easier.
>>
>>anvilsam
>>
>>_______________________________________________
>>http://mailman.qth.net/mailman/listinfo/theforge
>>theforge mail list group photo site is
>>http://www.photoaccess.com
>>Login:  [email protected]
>>password:  anvil
>>___________
>>
>>
>>
>>    
>>
>
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login:  [email protected]
>password:  anvil
>___________
>
>
>
>  
>