[TheForge] Nazel Question
gblacksmith
[email protected]
Thu Sep 11 10:48:01 2003
Ralph: Isn't Bob Bergman also the point of contact for the Turkish Sahinler
air-hammers as well? Grant
----- Original Message -----
From: "Ralph Sproul" <[email protected]>
To: <[email protected]>
Sent: Thursday, September 11, 2003 6:03 AM
Subject: Re: [TheForge] Nazel Question
> Grant, I call Bob Bergman who is the most reliable resource for the
hammers
> as he's done a lot of machining on them, and has outlets for rings,
leather,
> packings, guide plates, used motors, etc. He answers all my questions as
I
> come up with them. It is a real nice asset to have someone who's been in
> there before and has suppliers to contact. If you know Marc Krauss he may
> be able to help you if he's closer to you. He and Bob did the tape on
> rebuilding a hammer at Bob's shop.
>
> Bruce Wallace I've heard owns some rights to the Beaudry's and Nazel's -
or
> something like that, but I'm not familiar with what he actually has - so
> contacting him is another avenue to persue.
>
> Steve Howell also on theforge list is going thru a rebuild at the moment
and
> is dealing with sleeved bores, and tup repairs. We are currently
"chatting"
> on a couple questions about the hammers. It is the "brotherhood" and
> "networking" of us metalworkers that keeps it possible. Trying to start
> from scratch and hunt everything down yourself is a task. It's nice to
tap
> into folks who are doing it - or better yet - those who have done it
before.
>
> I'm just starting to rebuild mine(a 3B) I aquired from Bob in a trade in
on
> a Striker hammer sale close to me (about 100 miles south). I'll be much
> better informed ...................say around March or April........
:-)
>
> A good question is who else owns Nazels on the list? do you have parts
> availability lists made up? Would you care to share any resources?
>
> Ralph
>
> ----- Original Message -----
> From: "gblacksmith" <[email protected]>
> To: <[email protected]>
> Sent: Wednesday, September 10, 2003 8:25 PM
> Subject: Re: [TheForge] Nazel Question
>
>
> > Ralph: How difficult is it to get parts for Nazel hammers? Is there
any
> > sort of "support group" for owners of these hammers?
> >
> >
> > Grant
> > ----- Original Message -----
> > From: "Ralph Sproul" <[email protected]>
> > To: <[email protected]>
> > Sent: Wednesday, September 10, 2003 11:50 AM
> > Subject: Re: [TheForge] Nazel Question
> >
> >
> > > Bill, 1-800-Bob Bergman will be your best bet. :-)
> > >
> > > Bob has a tape on rebuilding a Nazel hammer that is
priceless -
> > that
> > > he did with Mark Krauss a few years back. It is one of the best ways
to
> > > understand this hammer, how to rebuild it, and the way it works. He
> also
> > > has literature on the Nazel I found to be very nice with parts names
and
> > > numbers (NOT that they are available any more), but just to realize
what
> > > your dealing with and how it goes together is a nice start.
> > > The tape and literature is worth whatever he is asking, it is
> > > informative and clear.
> > >
> > > Ralph
> > > ----- Original Message -----
> > > From: "Woolley" <[email protected]>
> > > To: <[email protected]>
> > > Sent: Wednesday, September 10, 2003 10:42 AM
> > > Subject: [TheForge] Nazel Question
> > >
> > >
> > > > Hello,
> > > >
> > > > Does anyone have any idea what is the best reference or source of
> > > > information for Nazel hammers? Sizes, dates of manufacture, parts
> > > > availability etc. Thanks.
> > > >
> > > > Regards,
> > > > Bill Woolley
> > > >
> > > >
> > > > _______________________________________________
> > > > http://mailman.qth.net/mailman/listinfo/theforge
> > > > theforge mail list group photo site is
> > > > http://www.photoaccess.com
> > > > Login: [email protected]
> > > > password: anvil
> > > > ___________
> > > >
> > > >
> > >
> > > _______________________________________________
> > > http://mailman.qth.net/mailman/listinfo/theforge
> > > theforge mail list group photo site is
> > > http://www.photoaccess.com
> > > Login: [email protected]
> > > password: anvil
> > > ___________
> > >
> > >
> > >
> >
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: [email protected]
> > password: anvil
> > ___________
> >
> >
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>