> So this brings to mind what I've seen in several tool making books:
> When you make a cold chisel, supposedly you finish forging by "packing" it
> as it passes critical. In other words, do the forging at the appropriate
> color and give it a few accurate whacks to further refine the grain while
> it's cooling.
> Any comments on this?
> I've noticed that P. Ross tends to do the final forging down into black to
> minimise scale and get the best finish, so I wonder if this also affects
> grain size.
> Also, all this discussion makes me want to just make tools out of S7 using
> the grinder, and forget the forge for that...
> Andy G.
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>
>
>